Читать книгу Animal Proteins - Hugh Garner Bennett - Страница 10
SECTION IV.—FINISHING PROCESSES
ОглавлениеAfter the tannage is complete, leather is hung up to dry. In the case of heavy leather this drying must be very carefully carried out in order to obtain a product of satisfactory appearance and saleable qualities. Associated with the drying are many mechanical operations (scouring and rolling) which assist very materially in imparting the desired qualities. After tanning, however, the quality of the final product is most strongly influenced by the amount of grease added in finishing. Some grease is always used in finishing, partly because even sole leather requires some measure of pliability and partly because a coating of oil over the leather during drying prevents the loose tannin from being drawn to the surface of the leather by capillarity, thereby causing dark and uneven patches and a "cracky" grain. The added grease is also a contribution to the "weight" of the finished article—a primary consideration for heavy leather, which is usually sold by weight. The finishing processes, indeed, tend to be dominated by this consideration, and become a series of efforts to retain as much tannin and add as much grease as are consistent with the requirements of the class of leather being manufactured. Sole leather does not contain more than about 2 per cent. grease, or its firmness is impaired. Belting leather, in which considerable pliability is needed, may contain about 9 per cent., whilst harness leather, which must be exceedingly tough and durable, may contain up to 13 per cent. of fatty matters. Upper leathers, which need to be soft and pliable as well as waterproof and durable, are very heavily "stuffed" and often contain up to 30-40 per cent. of grease. Sole leather is thus rather distinct from the rest, which are called "curried," "stuffed," or "dressed" leathers. The actual drying out before, after and between the various mechanical operations, each have an appropriate degree of wetness. In this country the drying is usually under the prevailing atmospheric conditions and is known as "weather drying." The goods are suspended by hooks or strings or by laying over poles in special sheds fitted with louvre boards by which the rate of drying can be roughly controlled. Weather drying is cheap, but exceedingly slow, and in unfavourable weather is very unreliable. The goods, moreover, need constant attention to obtain an even result. Steam pipes are usually laid along the shed floors, and are used in winter and damp weather to accelerate the drying, and also in the final shed stove to remove the last traces of moisture. Wet weather, however, will not stand a high temperature, and steam drying is better avoided when possible. Air-dried leather still contains about 14 per cent. of moisture. Many systems of shed ventilation have been suggested to hasten the drying and to secure a better control of the process. In one system a screw fan is fitted at one end of a shed (without louvre boards) and sucks air through the goods from an inlet at the other end. The air can be heated by a steam coil near the inlet. In another system a centrifugal fan blows air through an arrangement of pipes which distributes it to the drying sheds, and discharges it close to the floor by various branch pipes. The outlets are near the roof. A system of dampers permits hot air, warm air and the used wet air to be blended in the desired proportions. In America turret drying has been used. The sheds are vertically above one another and have latticed floors. Heated air is admitted at the bottom and rises through the goods up the building just as in a chimney. For many of the finishing operations it is important to obtain the leather in a uniformly half dry or "sammed" condition. This may be done by careful drying, and wetting back the parts that have become too dry with tepid water or weak sumac liquor, and then leaving the goods "in pile" until of uniform humidity. It may also be done by "wetting back" leather which has been completely dried out. There are also "samming machines" which by means of rollers squeeze out the excess liquor. Sole leather is dried out and finished immediately after tanning, but dressing leather is often "rough dried" out of tan liquors and wet back for finishing when required. Dressing leather is often treated in different factories; tanners selling it as rough leather and "curriers" finishing it.
Scouring is one of the first operations in finishing leather. The grain side is wet and worked with brushes and stones until the bloom and loose tannin are removed. This process aims at producing a good even colour and level surface, but is liable to cause a loss of weight. Dressing leather is often scoured on both grain and flesh, and weak soap or borax solutions are used to assist the process. In this operation hand labour has been now quite superseded by machine work. A great variety of machines have been devised. The mechanical working of leather takes place in various parts of finishing. These operations, known as "striking," "setting," "pinning," "jacking," may be carried out often by the same machine as used for scouring, but with a change of tool. The object of these operations is to get rid of wrinkles and creases, to produce softness, pliability and area, and to remove superfluous moisture, grease, dirt. The tools are of steel, brass, slate or vulcanite. Scouring is often effected by putting the goods into rotating drums together with extract and sumach. The bloom is removed by friction, the colour is improved by the sumach, whilst the extract keeps up the weight.
In finishing sole leather firmness is enhanced by "rolling." A brass roller passes to and fro over the goods with the exertion of considerable pressure. The operation is carried out by machinery.
Shaving is an important operation in the case of many dressing leathers. Its object is to produce a uniform thickness of the leather and an even surface on the flesh side. The sammed goods are laid over suitable beams and shaved with special sharp knives which possess a turned edge. This hand process, which demanded considerable skill, is fast becoming extinct, and machine shaving is already almost universal on account of its greater speed. The machines consist essentially of two rollers, one of which is smooth, whilst the other is a spiral knife-blade cylinder (cp. Section II., p. 23). The sammed goods are held in the hands and placed over the smooth roller, which is raised to the cutting roller by a foot treadle. A number of similar operations ("flatting," "whitening," "buffing") are carried out by a suitable change of tool. In all these operations good samming is important.
Splitting is another important operation on tanned leather. In this process the leather is cut parallel to its grain surface, thus yielding two pieces with the same area as the original, the "grain" and the "flesh split." It is essentially a machine operation, and is carried out by presenting the carefully sammed leather to a sharp knife-edge, towards which it must be constantly pressed. The "band-knife" machine is the most popular arrangement. The knife is an endless belt, which continually revolves round two pulley wheels of equal size. In between these the knife is horizontal, and is then used for splitting. The sammed leather is pushed towards the blade by two feed rollers, and the grain passes above the knife on to a small platform, whilst the flesh or "split" passes below and falls to the ground. Emery grinders and thick felt cleaners in the lower part of the machine keep the knife in good condition. The adjustment of the machine is delicate and requires considerable experience. With care splits may be obtained down to 1/16" thick, and sometimes as many as 6 or 7 splits are obtained from one hide.
Oiling is still usually done by hand, and cod oil is still preferred for many classes of goods. Of recent years there has been a great extension of the use of sulphonated oils, which have the valuable property of forming an emulsion with water or tan liquor. With these materials it is easier to ensure the goods being completely covered with oil. The penetration of the oil into the leather is also quicker and more complete. These oils have often the disadvantage of leaving solid fats on the exterior of the leather, which gives it an ugly smeared appearance.
Stuffing the dressing leathers is carried out in a variety of ways and with a variety of materials. The old process of hand stuffing employs a mixture of tallow and cod oil called "dubbin." This is made by melting the ingredients together and allowing them to cool with constant stirring to a nearly homogeneous salve. The dubbin is brushed thickly on to the flesh side of the sammed leather, which is then hung up to dry. As the moisture dries out the oils and soft fats penetrate the leather and leave the more solid fats on the outside. The proportions of tallow and oil are varied with the time of year and with the method of drying, for if the dubbin be too soft it will run off the leather, and if too hard will not penetrate it so well.
Drum stuffing is a more modern development in which a higher temperature is employed, about 140° F. The drum is heated up by steam or by hot air, and the sammed goods are then inserted and drummed for a few minutes until they are warmed. The drum is fitted with a heated funnel containing the melted grease, which is run in through the hollow axle. After a half to three-quarters of an hour's drumming the grease is completely absorbed by the leather. The drumming is continued for a while until the goods have cooled. Whilst still warm they are "set out" to remove creases and superfluous grease. Drum stuffing is not only quicker than hand stuffing, but also makes it possible to use the hard fats, and so make a leather which carries more grease without appearing greasy. Thus in drum stuffing, paraffin wax and wool fat are used, and their penetration assisted by small proportions of cod oil or dégras. If the leather be too wet the grease is not absorbed, whilst if it be drier than usual the leather will take more grease, but the resulting colour is not so good. There is also another method of stuffing which originates from the Continent. It is known as "burning in" and involves the use of still higher temperatures (195° to 212° F.). Wet leather will, of course, not stand this temperature, so that it is first necessary to make the leather absolutely dry. This is effected by drying in stoves at temperatures up to 110°-115° F. There are two ways in which the grease is applied. In one method the melted grease is poured by a ladle on to the flesh side and brushed over until evenly distributed. A second application of grease is made to the thicker parts. The hides are then put into warm water (120° F.) for about a quarter of an hour, and then drummed for half an hour. In the other method the goods are completely immersed in the melted fats for a few minutes in a steam-jacketer tank at a temperature of 195° F. After softening in water at 120° F. the goods are drummed. "Burning in" is used for the heavier dressing leathers such as belting and harness. It does not give good colour, but permits the employment of still more hard fats.
REFERENCES.
Procter, "Principles of Leather Manufacture," pp. 223, 378.
Bennett, "Manufacture of Leather," pp. 251-312.